MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Acclaim® 8200 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Acclaim 8200 polyol is a 8,000-molecular-weight diol based on propylene oxide.

Properties / Applications: This high-performance, low-monol polyether is prepared with Covestro's proprietary IMPACT™ technology, using a patented organo-metallic propoxylation catalyst. The terminal end-groups are predominantly secondary hydroxyls and have a relatively low reactivity. This polyol is acidified with a low level of phosphoric acid, making it suitable for use in isocyanate-terminated prepolymers. Acclaim 8200 polyol is used in polyurethane and other applications, including cast elastomers, sealants, epoxy flexibilizers, defoamers, lubricants, crude oil de-emulsifiers and plasticizers. As with any product, use of Acclaim 8200 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Acclaim 8200 polyol contains extremely low levels of monol. In some polyurethane systems, formulation changes, such as reducing the crosslinking level or changing the hard-segment content, may be necessary to maximize the benefits of using Acclaim polyols.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 0.950 g/cc
@Temperature 90.0 °C
0.950 g/cc
@Temperature 194 °F
 0.995 g/cc
@Temperature 30.0 °C
0.995 g/cc
@Temperature 86.0 °F
Bulk Density 1.01 g/cc0.0363 lb/in³
Viscosity 3000 cP3000 cP
 200 cP
@Temperature 80.0 °C
200 cP
@Temperature 176 °F
 1000 cP
@Temperature 48.0 °C
1000 cP
@Temperature 118 °F
Storage Temperature 20.0 - 60.0 °C68.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.020<= 0.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 190 °C374 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.030 %<= 0.030 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number13-15 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Acclaim® 2200 Polyol
Covestro Acclaim® 4200 Polyol
Covestro Baygal® 90 IK 51 Polyurethane
Covestro Acclaim® 4220N Polyol
BASF Pluracol® 2100 Slabstock HR Foam Polyol

PCOVEST0009 / 201792

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.