MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistance. TRA-BOND 789-3TN1 adhesive exhibits excellent bond strength to difficult-to-bond metals, such as gold and silver.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 37000 cP
@Temperature 25.0 °C
37000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 34.5 MPa5000 psiLap shear, alum to alum, @ 25°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 1000 Hz
4.2
@Frequency 1000 Hz
Dielectric Strength 31.5 kV/mm800 kV/in
Dissipation Factor 0.011
@Frequency 1000 Hz
0.011
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°FBelow Tg
 140 µm/m-°C77.8 µin/in-°FAbove Tg
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 126 °C259 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
Weight Loss % 0.28At 250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 868-3N1 Room Temperature Cure Adhesive
Tra-Con Tra-Bond 789-3T3N1 Moisture Resistant Adhesive
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive

PTRAC156 / 71084

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.