MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Riteflex® 440 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 440 is a nominal 40 Shore D thermoplastic polyester elastomer with medium modulus.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm0.012 - 0.014 in/inISO 294-4
Melt Flow 13.3 g/10 min
@Load 2.16 kg,
Temperature 220 °C
13.3 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292ISO 868
Hardness, Shore D 383815 sec; ISO 868
 3838ISO 868
Tensile Strength at Break 18.0 MPa2610 psi50mm/min; ISO 527-2/1A
 21.0 MPa3050 psiISO 527-1/2
Tensile Stress at Strain  2.00 MPa
@Strain 5.0 %
290 psi
@Strain 5.0 %
ISO 527-1/2
 4.00 MPa
@Strain 10 %
580 psi
@Strain 10 %
ISO 527-1/2
 7.00 MPa
@Strain 50 %
1020 psi
@Strain 50 %
ISO 727-1/2
 7.00 MPa
@Strain 50 %
1020 psi
@Strain 50 %
ISO 527-2/1A
 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
ISO 527-1/2
 12.7 MPa
@Strain 300 %
1840 psi
@Strain 300 %
ISO 527-1/2
Elongation at Break 650 %650 %50mm/min; ISO 527-2/1A
 650 %650 %ISO 527-1/2
Tensile Modulus 0.0550 GPa7.98 ksi50mm/min; ISO 527-2/1A
Flexural Strength 4.00 MPa580 psiISO 178
 2.00 MPa
@Strain 3.5 %
290 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.0450 GPa6.53 ksiISO 178
 0.0260 GPa
@Temperature 100 °C
3.77 ksi
@Temperature 212 °F
ISO 178
 0.270 GPa
@Temperature -40.0 °C
39.2 ksi
@Temperature -40.0 °F
ISO 178
Resilience 5858Bayshore, %
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Ross flex
Izod Impact, Notched (ISO) NBNBISO 180
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 96.0 kN/m548 pliISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+12 ohm-cm2.00e+12 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohm2.00e+15 ohmIEC 60093
Dielectric Constant 4.9
@Frequency 1e+6 Hz
4.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 240 µm/m-°C133 µin/in-°FISO 11359-2
Melting Point 195 °C383 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C117 °FISO 75-1, -2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 55.0 °C68.0 - 131 °Fcavity
 190 - 215 °C374 - 419 °Fhot runner
Feed Temperature 185 - 200 °C365 - 392 °F
Zone 1 185 - 200 °C365 - 392 °F
Zone 2 185 - 210 °C365 - 410 °F
Zone 3 185 - 210 °C365 - 410 °F
Zone 4 185 - 215 °C365 - 419 °F
Die Temperature 190 - 215 °C374 - 419 °F
Melt Temperature 190 - 215 °C374 - 419 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj\Blow\Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 2004-2 PBT, Unfilled
Celanese Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 655HS TPC, Unfilled
Celanese Riteflex® 447 TPC, Unfilled

PHCQ449 / 178904

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.