MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayflex® XGT-2 Polyurethane System, 50% BaSO4 Filled
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Bayflex XGT 2 is an elastomeric polyurethane system used in the reaction injection molding (RIM) process.

Properties / Applications: Bayflex XGT 2 is an elastomeric polyurethane system used in the reaction injection molding (RIM) process. The system is supplied as two liquid components: Component A is a modified diphenylmethane diisocyanate (MDI), and Component B is a polyether polyol system. The extended gel time of Bayflex XGT 2 gives equipment designers the flexibility to create large, complex parts that can be molded on existing injection machinery. The resin ’s soft feel and the ability to tailor part density through the addition of barium sulfate make this product ideal for applications that require some level of sound absorption, such as floor coverings in heavy trucks or equipment. In addition, the material is soft enough to be used for producing seals, gaskets and wire harness type applications. As with any product, use of the Bayflex XGT 2 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccIsocyanate (Component A)
 1.66 g/cc1.66 g/ccASTM D1622
 1.86 g/cc1.86 g/ccPolyol (Component B)
Viscosity 700 cP700 cPIsocyanate (Component A)
 8000 cP8000 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  78
@Time 5.00 sec
78
@Time 0.00139 hour
ASTM D2240
 80
@Time 1.00 sec
80
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 5.00 MPa725 psiperpendicular, 20 in/min, Die C; ASTM D412
 5.10 MPa740 psiparallel, 20 in/min, Die C; ASTM D412
 5.82 MPa
@Treatment Temp. 70.0 °C,
Time 252000 sec
844 psi
@Treatment Temp. 158 °F,
Time 70.0 hour
perpendicular, 20 in/min, Die C; ASTM D412
 5.87 MPa
@Treatment Temp. 70.0 °C,
Time 252000 sec
851 psi
@Treatment Temp. 158 °F,
Time 70.0 hour
parallel, 20 in/min, Die C; ASTM D412
Elongation at Break 247 %247 %perpendicular, 20 in/min, Die C; ASTM D412
 248 %248 %parallel, 20 in/min, Die C; ASTM D412
 268 %
@Treatment Temp. 70.0 °C,
Time 252000 sec
268 %
@Treatment Temp. 158 °F,
Time 70.0 hour
parallel, 20 in/min, Die C; ASTM D412
 282 %
@Treatment Temp. 70.0 °C,
Time 252000 sec
282 %
@Treatment Temp. 158 °F,
Time 70.0 hour
perpendicular, 20 in/min, Die C; ASTM D412
Tear Strength 4.24 kN/m24.2 pliparallel, Split Tear; ASTM D624
 5.28 kN/m30.1 pliperpendicular, Split Tear; ASTM D624
 16.5 kN/m94.3 pliparallel, Die C; ASTM D624
 17.2 kN/m97.9 pliperpendicular, Die C; ASTM D624
Compression Set 26.5 %26.5 %25% deflection; ASTM D3395
 
Thermal PropertiesMetricEnglishComments
Flash Point 114 °C237 °FPolyol (Component B)
 213 °C415 °FIsocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 66.0 - 77.0 °C151 - 171 °F
Moisture Content <= 0.90 %<= 0.90 %Polyol (Component B)
 
Descriptive Properties
Content22.6-23.1%NCO, Isocyanate (Component A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Miracll E180F Halogen-Free Flame Retardant TPU
BCC Products MB 1100 Polyurethane Foam Modeling Board
BCC Products Kwik Kast BC 8001 Urethane Casting
BCC Products BC 8660E Urethane Elastomer
BASF Elastollan® S 74 D TPUR

PCOVEST0136 / 201919

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.