System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celstran® PA66-SF6-02 PA66, 6% Stainless Steel Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Stainless Steel Filled; EMI Grade
Material Notes:
6% stainless steel reinforced nylon 6/6
6% stainless steel fiber reinforced, heat stabilized nylon 6/6
Celstran can be processed on a standard injection molding unit.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.19
g/cc
1.19
g/cc
ASTM D792
Density
1.19
g/cc
0.0430
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0040
cm/cm
0.0040
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.0050
cm/cm
0.0050
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
77.9
MPa
11300
psi
ASTM D638
80.0
MPa
11600
psi
5mm/min; ISO 527-2/1A
Elongation at Break
3.2 %
3.2 %
5mm/min; ISO 527-2/1A
2.9 %
@Temperature 22.8 °C
2.9 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus
3.60
GPa
522
ksi
1mm/min; ISO 527-2/1A
3.45
GPa
@Temperature 22.8 °C
500
ksi
@Temperature 73.0 °F
ASTM D638
Flexural Strength
125
MPa
18100
psi
ASTM D790
130
MPa
18900
psi
ISO 178
Flexural Modulus
3.20
GPa
464
ksi
ISO 178
3.45
GPa
@Temperature 22.8 °C
500
ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched
0.374
J/cm
0.700
ft-lb/in
ASTM D256
Charpy Impact, Notched
0.380
J/cm²
1.81
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
<=
1.0
ohm-cm
<=
1.0
ohm-cm
ASTM D257
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
76.7
°C
170
°F
ASTM D648
Processing Properties
Metric
English
Comments
Processing Temperature
70.0
-
80.0
°C
158
-
176
°F
80.0
-
100
°C
176
-
212
°F
Cavity temperature
Feed Temperature
20.0
-
50.0
°C
68.0
-
122
°F
Zone 1
285
-
295
°C
545
-
563
°F
Zone 2
290
-
300
°C
554
-
572
°F
Zone 3
300
-
310
°C
572
-
590
°F
Zone 4
300
-
315
°C
572
-
599
°F
Die Temperature
300
-
315
°C
572
-
599
°F
Melt Temperature
290
-
315
°C
554
-
599
°F
Mold Temperature
75.0
-
85.0
°C
167
-
185
°F
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Moisture Content
0.18 %
0.18 %
Necessary low maximum residual
Dew Point
<=
-30.0
°C
<=
-22.0
°F
Pre-drying
Descriptive Properties
Injection molding
Yes
Longer pre-drying times/storage
Material can be over dried and may discolor.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Avient Stat-Tech™ NN-30GF-15SS Nylon 6/6 - 30% Glass Fiber - 15% Stainless Steel
Celanese Celstran® PA66-SF10-02 PA66, 10% Stainless Steel Reinforced
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled
Avient Stat-Tech™ NN-05SS/000 Nylon 6/6 - 5% Stainless Steel Fiber
RTP Company EMI 261 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
PHCR167 / 158736
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.