Product Description: FRblend® PC-1303 is a 10% glass fiber reinforced, flame retardant polycarbonate compounds comply with UL 94 V-0 rating at 1.6mm thickness. Features: - Flame retardant
- Balance of strength
Uses:- Electrical/electronic components
Forms:Processing Method:Information provided by Colour Image Plastic Compound Sdn Bhd |