MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 1301-7815 Polyphenylene sulfide, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: Polyphenylene sulfide, linear with carbon fibers, lubricant modified, grey

Main features: Improved friction and wear behavior, self-lubricating, for highest tribological requirements. High-strength and stiffness parts with low creep. Electrically conductive, suitable for continuous discharging of statically-generated electricity. High continuous use and heat-distortion temperatures. Non flammable.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.65 g/cc1.65 g/ccISO 1183-3
Water Absorption <= 0.0500 %
@Time 86400 sec
<= 0.0500 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.00200 - 0.00500 cm/cm0.00200 - 0.00500 in/inDIN 16742
Melt Flow 11.55 g/10 min
@Load 2.16 kg,
Temperature 300 °C
11.55 g/10 min
@Load 4.76 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 135 MPa19600 psi50 mm/min; ISO 527
Elongation at Break 1.20 %1.20 %50 mm/min, Fmax; ISO 527
Tensile Modulus 15.0 GPa2180 ksi1 mm/min; ISO 527
Flexural Strength 175 MPa25400 psi10 mm/min; ISO 178
Flexural Modulus 14.0 GPa2030 ksi2 mm/min; ISO 178
Flexural Strain at Break 1.30 %1.30 %10 mm/min, Fmax; ISO 178
Charpy Impact Unnotched 1.80 J/cm²8.57 ft-lb/in²80x10x4mm; ISO 179 1eU
Coefficient of Friction 0.270
@Pressure 4.00 MPa
0.270
@Pressure 580 psi
100Cr6, 13 m/s; Block on Ring; ASTM G137
K (wear) Factor  300 x 10-8 mm³/N-M
@Pressure 4.00 MPa
149 x 10-10 in³-min/ft-lb-hr
@Pressure 580 psi
Sp. Wear Rate-Block on Ring, vs. 100Cr6, 1 m/s; ASTM G137
 480 x 10-8 mm³/N-M
@Pressure 4.00 MPa
238 x 10-10 in³-min/ft-lb-hr
@Pressure 580 psi
Sp. Wear Rate-Block on Ring, vs. 100Cr6, 1 m/s; ASTM G137
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air  220 °C
@Time 7.20e+7 sec
428 °F
@Time 20000 hour
Continuous; IEC 60216
 240 °C
@Time 720000 sec
464 °F
@Time 200 hour
during lifetime
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °F80x10x4mm; ISO 75
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 340 °C608 - 644 °F
Zone 1 300 - 320 °C572 - 608 °F
Zone 2 310 - 330 °C590 - 626 °F
Zone 3 320 - 340 °C608 - 644 °F
Melt Temperature 330 °C626 °F
Mold Temperature 150 - 180 °C302 - 356 °F
Drying Temperature  50.0 - 90.0 °C
@Time <=14400 sec
122 - 194 °F
@Time <=4.00 hour
Dehumidifying
 100 - 140 °C
@Time 7200 - 14400 sec
212 - 284 °F
@Time 2.00 - 4.00 hour
Dehumidifying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8715 / 325099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.