MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tin Die-Casting Alloy (UNS L13913)
Categories: Metal; Nonferrous Metal; Tin Alloy

Key Words: ASTM B102 (CY44A), Babbitt Alloy 1 (White Metal)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.34 g/cc0.265 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 171710 mm ball/500 kg load-30 sec.
Tensile Strength, Ultimate 62.0 MPa8990 psiDie Cast
 64.0 MPa9280 psiChill Cast
Elongation at Break 2.0 %2.0 %in 50 mm
Modulus of Elasticity 50.0 GPa7250 ksi
Compressive Yield Strength 30.3 MPa4390 psi
Ultimate Compressive Strength 88.6 MPa12900 psi
Izod Impact 3.40 J2.51 ft-lbChill Cast
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 - 371 °C433 - 700 °F
Solidus 223 °C433 °F
Liquidus 371 °C700 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.010 %<= 0.010 %
Antimony, Sb 4.0 - 5.0 %4.0 - 5.0 %
Arsenic, As <= 0.080 %<= 0.080 %
Copper, Cu 4.0 - 5.0 %4.0 - 5.0 %
Iron, Fe <= 0.080 %<= 0.080 %
Lead, Pb <= 0.35 %<= 0.35 %
Tin, Sn 90 - 92 %90 - 92 %
Zinc, Zn <= 0.010 %<= 0.010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin Die Casting Alloy (UNS L13650)
Tin Die Casting Alloy (UNS L13820)
60-40 Soft Solder (60 Sn-40Pb) Tin-Lead Soft Solder (UNS L13600)
60-40 Soft Solder (60 Sn-40Pb) (UNS L13601)
Aluminum 384.0-F Die Casting Alloy

MLS13913 / 205656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.