MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® MS PC+ASA 5008 ASUV 14065 PC+ASA
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Base Polymer: Polycarbonate + Acrylonitrile Styrene Acrylate Blend

Filler/Additive System: antistatic-permanent, UV stabilized

Special Features: good chemical resistance, good weathering resistance

Market Segment: Automotive, Electrical and Electronic

Application Area: injection molded parts

Typical Applications: Interior decoration/finishing, housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Melt Flow 39 g/10 min
@Load 5.00 kg,
Temperature 260 °C
39 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 47.0 MPa6820 psiISO 527
Tensile Modulus 1.85 GPa268 ksiISO 527
Flexural Strength 67.0 MPa9720 psiISO 178
Flexural Modulus 1.95 GPa283 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1/-2
Vicat Softening Point 113 °C235 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 300 °C500 - 572 °FInjection molding
Mold Temperature 60.0 - 100 °C140 - 212 °FInjection molding
Drying Temperature  90.0 - 115 °C
@Time 7200 - 14400 sec
194 - 239 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 90.0 - 115 °C
@Time 14400 - 28800 sec
194 - 239 °F
@Time 4.00 - 8.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolycarbonate + Acrylonitrile Styrene Acrylate Blend

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers ELIX ABS E401 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade
INEOS Styrolution Terluran® EHI-4 NR ABS Extrusion Application
A. Schulman Diamond ASA S150
A. Schulman Diamond ASA S140
A. Schulman Diamond ASA T-105

PALBIS8080 / 242139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.