MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Overview of materials for Solder/Braze Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Solder/Braze Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.750 - 19.1 g/cc0.0271 - 0.689 lb/in³Average value: 7.81 g/cc Grade Count:867
Water Absorption 5.00 - 35.0 %5.00 - 35.0 %Average value: 22.5 % Grade Count:4
pH 0.000 - 12.00.000 - 12.0Average value: 4.24 Grade Count:58
Viscosity 2150 - 750000 cP2150 - 750000 cPAverage value: 281000 cP Grade Count:21
Surface Tension 32.0 - 54.0 dynes/cm32.0 - 54.0 dynes/cmAverage value: 34.5 dynes/cm Grade Count:17
 
Chemical PropertiesMetricEnglishComments
Acid Value 12.0 - 93612.0 - 936Average value: 115 Grade Count:26
Total Acid Number 15.0 - 65.015.0 - 65.0Average value: 33.6 Grade Count:16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 0.900 - 40.00.900 - 40.0Average value: 12.9 Grade Count:67
Hardness, Knoop 1000 - 23001000 - 2300Average value: 1350 Grade Count:4
Hardness, Vickers 12.9 - 16.112.9 - 16.1Average value: 15.4 Grade Count:4
Tensile Strength, Ultimate 1.90 - 2000 MPa276 - 290000 psiAverage value: 209 MPa Grade Count:295
Tensile Strength, Yield 10.0 - 907 MPa1450 - 132000 psiAverage value: 314 MPa Grade Count:44
Elongation at Break 0.000 - 200 %0.000 - 200 %Average value: 27.0 % Grade Count:171
Modulus of Elasticity 10.0 - 150 GPa1450 - 21800 ksiAverage value: 42.2 GPa Grade Count:47
Compressive Yield Strength 69.0 - 758 MPa10000 - 110000 psiAverage value: 321 MPa Grade Count:13
Poissons Ratio 0.330 - 0.4000.330 - 0.400Average value: 0.374 Grade Count:11
Shear Modulus 11.0 - 12.0 GPa1600 - 1740 ksiAverage value: 11.5 GPa Grade Count:6
Shear Strength 2.07 - 276 MPa300 - 40000 psiAverage value: 49.9 MPa Grade Count:57
Adhesive Bond Strength 11.0 - 30.0 MPa1600 - 4350 psiAverage value: 19.0 MPa Grade Count:13
Izod Impact 19.0 - 27.1 J14.0 - 20.0 ft-lbAverage value: 21.5 J Grade Count:12
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000164 - 0.000784 ohm-cm0.00000164 - 0.000784 ohm-cmAverage value: 0.0000212 ohm-cm Grade Count:340
Surface Resistance 0.00250 - 3.50e+12 ohm0.00250 - 3.50e+12 ohmAverage value: 1.17e+12 ohm Grade Count:5
Insulation Resistance 3.76e+9 - 8.11e+13 ohm3.76e+9 - 8.11e+13 ohmAverage value: 1.38e+13 ohm Grade Count:16
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 - 40.0 µm/m-°C6.67 - 22.2 µin/in-°FAverage value: 23.2 µm/m-°C Grade Count:202
Specific Heat Capacity 0.126 - 0.272 J/g-°C0.0301 - 0.0650 BTU/lb-°FAverage value: 0.179 J/g-°C Grade Count:29
Thermal Conductivity 2.00 - 418 W/m-K13.9 - 2900 BTU-in/hr-ft²-°FAverage value: 58.8 W/m-K Grade Count:132
Melting Point -10.0 - 1700 °C14.0 - 3090 °FAverage value: 511 °C Grade Count:1004
Solidus 11.0 - 1420 °C51.8 - 2590 °FAverage value: 498 °C Grade Count:943
Liquidus 11.0 - 1450 °C51.8 - 2630 °FAverage value: 543 °C Grade Count:939
Boiling Point 78.3 - 2210 °C173 - 4010 °FAverage value: 466 °C Grade Count:14
Maximum Service Temperature, Air 88.0 - 1540 °C190 - 2800 °FAverage value: 433 °C Grade Count:77
Working Point 450 - 1300 °C842 - 2370 °FAverage value: 732 °C Grade Count:19
Minimum Service Temperature, Air 593 °C1100 °FAverage value: 593 °C Grade Count:4
Flash Point 11.0 - 285 °C51.8 - 545 °FAverage value: 49.9 °C Grade Count:57
 
Processing PropertiesMetricEnglishComments
Processing Temperature 93.0 - 1230 °C199 - 2250 °FAverage value: 654 °C Grade Count:258
Moisture Content 1.00 - 35.0 %1.00 - 35.0 %Average value: 23.6 % Grade Count:8
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00100 - 95.0 %0.00100 - 95.0 %Average value: 10.2 % Grade Count:107
Antimony, Sb 0.000400 - 10.0 %0.000400 - 10.0 %Average value: 1.86 % Grade Count:124
Arsenic, As 0.000500 - 2.00 %0.000500 - 2.00 %Average value: 0.0832 % Grade Count:60
Bismuth, Bi 0.000100 - 100 %0.000100 - 100 %Average value: 26.4 % Grade Count:198
Boron, B 0.0100 - 18.0 %0.0100 - 18.0 %Average value: 2.72 % Grade Count:33
Cadmium, Cd 0.000100 - 95.0 %0.000100 - 95.0 %Average value: 11.2 % Grade Count:156
Carbon, C 0.00500 - 0.900 %0.00500 - 0.900 %Average value: 0.0628 % Grade Count:48
Chromium, Cr 0.0700 - 20.0 %0.0700 - 20.0 %Average value: 11.7 % Grade Count:28
Cobalt, Co 0.0500 - 50.8 %0.0500 - 50.8 %Average value: 7.68 % Grade Count:19
Copper, Cu 0.0100 - 100 %0.0100 - 100 %Average value: 31.4 % Grade Count:469
Gallium, Ga 0.400 - 100 %0.400 - 100 %Average value: 24.4 % Grade Count:12
Germanium, Ge 0.0100 - 55.0 %0.0100 - 55.0 %Average value: 10.4 % Grade Count:14
Gold, Au 10.0 - 99.8 %10.0 - 99.8 %Average value: 62.6 % Grade Count:115
Indium, In 0.0500 - 100 %0.0500 - 100 %Average value: 35.1 % Grade Count:152
Iridium, Ir 0.100 - 0.300 %0.100 - 0.300 %Average value: 0.157 % Grade Count:7
Iron, Fe 0.00100 - 40.0 %0.00100 - 40.0 %Average value: 1.39 % Grade Count:101
Lead, Pb 0.00200 - 100 %0.00200 - 100 %Average value: 49.0 % Grade Count:403
Lithium, Li 0.150 - 0.500 %0.150 - 0.500 %Average value: 0.284 % Grade Count:5
Magnesium, Mg 0.0700 - 0.150 %0.0700 - 0.150 %Average value: 0.107 % Grade Count:3
Manganese, Mn 0.0000500 - 39.5 %0.0000500 - 39.5 %Average value: 9.70 % Grade Count:43
Molybdenum, Mo 0.750 - 4.00 %0.750 - 4.00 %Average value: 2.08 % Grade Count:3
Nickel, Ni 0.00100 - 94.6 %0.00100 - 94.6 %Average value: 23.0 % Grade Count:171
Oxygen, O 0.000500 - 1.00 %0.000500 - 1.00 %Average value: 0.213 % Grade Count:5
Palladium, Pd 3.00 - 76.0 %3.00 - 76.0 %Average value: 22.5 % Grade Count:50
Phosphorus, P 0.000300 - 12.0 %0.000300 - 12.0 %Average value: 3.19 % Grade Count:88
Platinum, Pt 0.400 - 5.00 %0.400 - 5.00 %Average value: 1.88 % Grade Count:6
Selenium, Se 0.000300 - 0.00500 %0.000300 - 0.00500 %Average value: 0.00461 % Grade Count:12
Silicon, Si 0.0100 - 19.0 %0.0100 - 19.0 %Average value: 4.51 % Grade Count:62
Silver, Ag 0.00200 - 100 %0.00200 - 100 %Average value: 32.5 % Grade Count:474
Sulfur, S 0.00150 - 0.0200 %0.00150 - 0.0200 %Average value: 0.0185 % Grade Count:12
Tin, Sn 0.000200 - 100 %0.000200 - 100 %Average value: 38.6 % Grade Count:480
Titanium, Ti 0.0500 - 70.0 %0.0500 - 70.0 %Average value: 7.07 % Grade Count:28
Zinc, Zn 0.000100 - 98.3 %0.000100 - 98.3 %Average value: 15.7 % Grade Count:305
Zirconium, Zr 0.0500 %0.0500 %Average value: 0.0500 % Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Copper Alloy
Overview of materials for Aluminum Alloy
Overview of materials for Nickel Alloy
Overview of materials for Zinc Alloy
60-40 Soft Solder (60 Sn-40Pb) - ASTM B 32 Grade Sn60

M01068 / 81677

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.