MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa PC-S609 Toughened PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes:
    Features:
  • Good mechanical properties
  • Super high impact strength
  • Good weather resistance
  • High gloss
  • Good processing properties
  • Stress cracking properties

    Applications:
  • OA and IT parts
  • Automobile accessories
  • Electrical and electronic parts
  • Switch and plug
  • Household appliance

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc
@Temperature 23.0 °C
1.19 g/cc
@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
0.0050 - 0.0070 in/in
@Temperature 73.4 °F
ASTM D955
Melt Flow 12 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
12 - 16 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.0 MPa8410 psi50mm/min; ASTM D638
Elongation at Break >= 60 %>= 60 %50mm/min; ASTM D638
Flexural Strength 82.0 MPa11900 psi2mm/min; ASTM D790
Flexural Modulus 2.30 GPa334 ksi2mm/min; ASTM D790
Izod Impact, Notched >= 4.50 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 8.43 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm,
Temperature 23.0 °C
NB
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
@Thickness 6.40 mm
268 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
@Thickness 6.40 mm
257 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 275 °C<= 527 °F
Rear Barrel Temperature 240 - 270 °C464 - 518 °FStart Point: 240°C
Middle Barrel Temperature 240 - 260 °C464 - 500 °FStart Point: 235°C
Front Barrel Temperature 250 - 260 °C482 - 500 °FStart Point: 240°C
Melt Temperature 240 - 280 °C464 - 536 °FStart Point: 250°C
Mold Temperature 40.0 - 80.0 °C104 - 176 °FStart Point: 60°C
Drying Temperature 100 - 115 °C
@Time 10800 - 14400 sec
212 - 239 °F
@Time 3.00 - 4.00 hour
Pre-dry
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
 
Descriptive Properties
Injection Speed60-90%
Weather Resistance (delta E)ASTM D4459; 200hr xenon lamp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 1899 Polycarbonate, Impact Grade
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
LG Chemical LUPOY SC1004L PC, High Impact
Kingfa JH820 Modified PC
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE

PKINGF087 / 104346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.