MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Braskem HF3712 Extrusion Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Description: The HF3712 resin is a Linear Low Density Polyethylene(1), produced through slurry loop process and indicated for the production of geomembranes. It shows excellent resistance to environmental stress cracking (ESCR), good processability and melt strength.

Additive: Lubricant – Antioxidant.

Application: Geomembranes.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1500 hour>= 1500 hourSP-NCTL; ASTM D5397
ESCR 10% Igepal® 1500 hour
@Temperature 50.0 °C
1500 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow 10.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 1289 %1289 %ASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus, 1% Secant 682 MPa98900 psiASTM D790
Izod Impact, Notched 7.35 J/cm13.8 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C129 °FASTM D648
Vicat Softening Point 62.0 °C
@Load 5.10 kg
144 °F
@Load 11.2 lb
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade
Braskem AC59 HDPE Monofilament Polyethylene Homopolymer

PBRASK2107 / 199988

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.