MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT QSil 212 Transparent Liquid Silicone Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: The product is a transparent and colorless silicone formulation and is ideal for optical applications. The viscosity profile enables excellent flow around components and is excellent for potting complex parts. The chemical composition results in a cured product that is hydrolytically stable as well as reversion resistant. The silicone elastomer provides electrical insulation and physical shock resistance of components and enables environmental protection.

Key Features

  • UL listed in file No. E205830
  • Low linear shrinkage
  • Non-yellowing catalyst system
  • Chemical adhesion with use of primer
Application: LED encapsulation

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³A
 1.00 g/cc0.0361 lb/in³B
Brookfield Viscosity 3000 cP3000 cPB
 6500 cP6500 cPMixed
 10000 cP10000 cPA
Storage Temperature <= 38.0 °C<= 100 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240-95
Tensile Strength 8.62 MPa1250 psiISO 37
Elongation at Break 120 %120 %ISO 37
Tear Strength 4.38 kN/m25.0 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cmASTM D-257
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.411.41
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 125 °C
0.167 hour
@Temperature 257 °F
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Pot Life 15.0 min15.0 min
Gel Time 60.0 min60.0 min
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceAddition
ColorTransparent and colorlessA
 Transparent and colorlessB
 Transparent and colorlessCured Product
Mix Ratio1:1By Weight
RheologyLiquid, Newtonian

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL056 / 314539

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.