MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Colour Image Plastic Compound Smoothblend® POM-3500 POM, 25% Glass Bead Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Glass Bead Filled

Material Notes: Product Description: Smoothblend® POM-3500 is a glass bead filled polyacetal compound offering high mechanical and thermal properties.

Features:

  • Glass bead filled, 25%
  • Good wear resistance
  • Good mechanical & thermal
Uses:
  • Mechanical parts
  • Automotive applications
  • Plastic gears
  • Bushing & sliding components
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
@Thickness 3.20 mm
0.015 - 0.020 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Strength 70.0 MPa10200 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
@Thickness 4.00 mm
293 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 185 °C356 - 365 °F
Middle Barrel Temperature 185 - 190 °C365 - 374 °F
Front Barrel Temperature 190 - 200 °C374 - 392 °F
Nozzle Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 180 - 215 °C356 - 419 °F
Mold Temperature 80.0 - 105 °C176 - 221 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
 <= 6.00 hour<= 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO037 / 265929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.