MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Stainless Steel Filled; EMI Grade

Material Notes: EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Linear Mold Shrinkage, Flow 0.0050 - 0.0065 cm/cm0.0050 - 0.0065 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm0.0070 - 0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi
Elongation at Break 1.5 %1.5 %
Tensile Modulus 11.0 GPa1600 ksi
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 200 ohm-cm200 ohm-cm
Surface Resistance 20 ohm20 ohm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °F
Vicat Softening Point 245 °C
@Load 5.00 kg
473 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 300 °C527 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
 
Descriptive Properties
Electromagnetic reflection90 dB
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Edinburg Plastics DTG675 PA 6/6 Impact Modified, 25% Glass Filled
Celanese Celstran® PA66-SF6-02 PA66, 6% Stainless Steel Reinforced
Avient Stat-Tech™ NN-30GF-15SS Nylon 6/6 - 30% Glass Fiber - 15% Stainless Steel
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled

PLATH9968 / 177664

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.