MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.

Data provided by the manufacturer, Solvay Advanced Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³DAM; ISO 1183
Filler Content 40 %40 %Glass
Water Absorption 0.21 %0.21 %24 hr (DAM); ISO 62
Moisture Absorption at Equilibrium 1.5 %1.5 %65% RH (beginning DAM); Solvay Test
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inSolvay Test
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 9.50 GPa1380 ksiISO 527
Flexural Strength 210 MPa30500 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inISO 180
Izod Impact, Unnotched 7.50 J/cm14.1 ft-lb/inISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °F
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 280 °C482 - 536 °F
Rear Barrel Temperature 250 - 280 °C482 - 536 °FCompression Zone
Middle Barrel Temperature 250 - 280 °C482 - 536 °FHomogenization Zone
Front Barrel Temperature 260 - 290 °C500 - 554 °FNozzle Zone
Melt Temperature <= 270 °C<= 518 °F
Mold Temperature 120 - 140 °C248 - 284 °FNeeded to develop high crystallinity
Injection Pressure 50.0 - 250 MPa7250 - 36300 psi
Hold Pressure 30.0 - 150 MPa4350 - 21800 psi
Back Pressure 0.000 - 1.00 MPa0.000 - 145 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLN9f / 68331

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.