MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material with high molecular weight, high crystallinity and very low inner stress level. Zellamid® 1200 G is showing significant low moisture absorption, superior dimensional stability combined with high impact strength even at low temperatures and an excellent chemical resistance.

Zellamid® 1200 G is the ideal longterm solution for bushes, bearings, rollers and gear wheels subjected to high load and wear demanding for dimensional stability particularly when exposed to high humidity and water.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³Dry Density
Moisture Absorption at Equilibrium 0.90 %0.90 %50% RH
Water Absorption at Saturation 1.4 %1.4 %23°C
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.050 - 0.100.050 - 0.10to steel, added lubrication
 0.400.40to steel, no lubrication; ISO/DTR 7147
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 - 3.00e+13 ohm-cm1.00e+13 - 3.00e+13 ohm-cmDIN 53482
Surface Resistance 1.00e+15 - 3.00e+15 ohm1.00e+15 - 3.00e+15 ohmDIN 53482
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength 50.0 kV/mm1270 kV/inDIN 53481
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52612
Melting Point 190 °C374 °F
Maximum Service Temperature, Air 110 °C230 °Flong time operation
 130 °C266 °Fmedium time operation
 150 °C302 °Fa few hours operation
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZELL21 / 72950

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.