MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Cookson Group Plaskon® SMT-B-1NLV Molding Compound for PBGAs  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is an epoxy molding compound optimized specifically for PBGA applications with no plasma cleaning required before molding. It has the same unique resin system as the SMT-B-1, which minimizes warpage and enables trouble-free molding onto rigid and flexible laminate substrates. Minimal dimensional change after molding, post bake and subsequent solder treatment make this compound an excellent choice for PBGA and CSP applications.

Features:

  • Faster cure speed
  • Improved warp performance
  • Lower viscosity
  • No plasma cleaning required before molding

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.88 g/cc1.88 g/cc
Viscosity 4400 cP
@Temperature 175 °C
4400 cP
@Temperature 347 °F
Automatic orifice, at 1000 psi
Spiral Flow 158 cm62.2 inat 175°C and 1000 psi
Ash 78 %78 %
Storage Temperature <= 5.00 °C<= 41.0 °FRecommended
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272Cull hot
Flexural Strength 108.9 MPa15790 psi
 58.84 MPa
@Temperature 215 °C
8534 psi
@Temperature 419 °F
Flexural Modulus 16.87 GPa2446 ksi
 10.10 GPa
@Temperature 215 °C
1465 ksi
@Temperature 419 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.30e+16 ohm-cm
@Temperature 22.0 °C
5.30e+16 ohm-cm
@Temperature 71.6 °F
Dielectric Constant 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
Dissipation Factor 0.0035
@Frequency 1000 Hz
0.0035
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 20.0 °C
8.89 µin/in-°F
@Temperature 68.0 °F
Alpha 1
 59.0 µm/m-°C
@Temperature 20.0 °C
32.8 µin/in-°F
@Temperature 68.0 °F
Alpha 2
Thermal Conductivity 0.860 W/m-K5.97 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 228 °C442 °F
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Oxygen Index 32 %32 %
 
Processing PropertiesMetricEnglishComments
Mold Temperature 175 °C347 °F
Back Pressure 5.52 - 8.27 MPa800 - 1200 psi
Cure Time 1.17 - 2.50 min0.0194 - 0.0417 hourIn mold
 240 - 720 min
@Temperature 175 °C
4.00 - 12.0 hour
@Temperature 347 °F
Post mold
Gel Time 0.333 min0.333 minRam follower, at 175°C and 1000 psi
Shelf Life 0.100 Month0.100 Monthat 35°C, <40% loss of spiral flow
 0.250 Month0.250 Monthat 21°C, <40% loss of spiral flow
 24.0 Month24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Hydrolyzable Halides<1 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLASK005 / 56295

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.