Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Process: Injection Molding Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |