Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materials and its ecoprofile is very favorable when compared to similar products based on crude oil. The main features of Grilamid XE 4104 black 9992 are:- Low water absorption
- Good heat, UV and chemical resistance
- Easy processing
Grilamid XE 4104 black 9992 is particularly suitable for the manufacturing of technical injection molded parts in the application fields of:- Automotive
- Electrical & Electronic goods
- Mechanical engineering
- Sports & leisure goods
- Domestic appliances
Information provided by EMS Grivory |