MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllium PF-60, Foil Grade
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Pure Element

Material Notes: Composition listed is reported for product available from Materion Corporation (formerly Brush Wellman). Property data below is typical of pure Be - not necessarily grade PF-60.

Beryllium foil is manufactured by rolling at elevated temperature. Rolling creates anisotropy in the product, so multi-directional rolling techniques are often used. Be foil is used in radiation detectors and sources.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

General beryllium information: Beryllium is one of the lightest metals and has a high strength-to-weight ratio, stiffness-to-weight ratio, and very high specific heat, thermal conductivity, and heat of fusion. It has significant ductility, is readily machined and can be rolled, drawn, or extruded. It finds applications in nuclear reactors (neutron moderator and reflector), X-ray sources/detectors (X-ray transparency), IR target acquisition systems, inertial guidance instruments, computer parts, other aircraft and satellite structures, and heat sink constraining cores. Beryllium is usually produced via a powder metallurgy process to improve machinability and mechanical properties.

Information provided by Materion Corporation (formerly Brush Wellman) and the references.

Key Words: Brush Wellman; PF60 Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.844 g/cc0.06662 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 303 GPa43900 ksi
Poissons Ratio 0.070 - 0.180.070 - 0.18values between 0.07 and 0.18 have been reported for beryllium
Shear Modulus 135 GPa19600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000430 ohm-cm0.00000430 ohm-cm
Magnetic Susceptibility -1.00e-6-1.00e-6cgs/g
Critical Superconducting Temperature 0.0260 K0.0260 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1133 J/g487.4 BTU/lbBe has an unusually high heat of fusion.
CTE, linear  11.5 µm/m-°C
@Temperature 25.0 °C
6.39 µin/in-°F
@Temperature 77.0 °F
increases rapidly until 100°C
 14.5 µm/m-°C
@Temperature 25.0 - 300 °C
8.06 µin/in-°F
@Temperature 77.0 - 572 °F
 16.5 µm/m-°C
@Temperature 25.0 - 600 °C
9.17 µin/in-°F
@Temperature 77.0 - 1110 °F
 18.4 µm/m-°C
@Temperature 25.0 - 1000 °C
10.2 µin/in-°F
@Temperature 77.0 - 1830 °F
Specific Heat Capacity 1.925 J/g-°C0.4601 BTU/lb-°F
Thermal Conductivity 216 W/m-K1500 BTU-in/hr-ft²-°F
Melting Point 1273 - 1283 °C2323 - 2341 °F
Boiling Point 2471 °C4480 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.610.61650 nm
Reflection Coefficient, Visible (0-1) 0.500.5050% visible; 55% UV; 98% IR (10.6 µm)
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.050 %<= 0.050 %
BeO <= 0.80 %<= 0.80 %
Beryllium, Be >= 99 %>= 99 %
Boron, B <= 0.00030 %<= 0.00030 %
Cadmium, Cd <= 0.00020 %<= 0.00020 %
Calcium, Ca <= 0.010 %<= 0.010 %
Carbon, C <= 0.070 %<= 0.070 %
Chromium, Cr <= 0.010 %<= 0.010 %
Cobalt, Co <= 0.0010 %<= 0.0010 %
Copper, Cu <= 0.010 %<= 0.010 %
Iron, Fe <= 0.070 %<= 0.070 %
Lead, Pb <= 0.0020 %<= 0.0020 %
Lithium, Li <= 0.00030 %<= 0.00030 %
Magnesium, Mg <= 0.050 %<= 0.050 %
Manganese, Mn <= 0.012 %<= 0.012 %
Molybdenum, Mo <= 0.0020 %<= 0.0020 %
Nickel, Ni <= 0.020 %<= 0.020 %
Nitrogen, N <= 0.040 %<= 0.040 %
Silicon, Si <= 0.040 %<= 0.040 %
Silver, Ag <= 0.0010 %<= 0.0010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium IF-1, Foil Grade
Beryllium, Be
Beryllium I-70B, Vacuum Hot Pressed
Beryllium IP-70, Powder
Beryllium I-220C, Vacuum Hot Pressed

MBEPF6 / 10289

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.