Description: Sealant tape. Ideally suited to aerospace applications. Features & Benefits: - Predominantly used as a debulk tape in aerospace applications
- Low tack for ease of bag repositioning
- Strips cleaning and quickly after curing, on cooling below 66°C (151°F)
- Manufactured by Schnee Morehead in the USA.
Information provided by Cytec, subsequently acquired by Solvay. |