MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning HPFS® 7980 KrF High Purity Fused Silica
Categories: Ceramic; Glass; Optical

Material Notes: Glass HPFS® 7980 is a high purity non-crystalline silica glass with excellent optical qualities. Product characteristics include extraordinary low refractive index variations leading to state-of-the-art homogeneity values, low birefringence, exceptional transmittance from the deep ultraviolet through the infrared region, and an ultra-low thermal expansion coefficient. HPFS® 7980 KrF Grade is UV laser resistant.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 522522kg/mm² (100 g load)
Tensile Strength 54.0 MPa7830 psi
Modulus of Elasticity 73.00 GPa10590 ksi
Modulus of Rupture 0.0524 GPa7.60 ksiabraded
Compressive Strength 1140 MPa165000 psi
Bulk Modulus 35.9 GPa5210 ksi
Poissons Ratio 0.160.16
Shear Modulus 31.0 GPa4500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.480 µm/m-°C
@Temperature -100 - 100 °C
0.267 µin/in-°F
@Temperature -148 - 212 °F
 0.520 µm/m-°C
@Temperature 5.00 - 35.0 °C
0.289 µin/in-°F
@Temperature 41.0 - 95.0 °F
 0.570 µm/m-°C
@Temperature 0.000 - 200 °C
0.317 µin/in-°F
@Temperature 32.0 - 392 °F
Specific Heat Capacity 0.770 J/g-°C0.184 BTU/lb-°F
Thermal Conductivity 1.38 W/m-K9.58 BTU-in/hr-ft²-°F
Softening Point 1590 °C2890 °F107.6 Poise
Annealing Point 1040 °C1910 °F1013 Poise
Strain Point 893 °C1640 °F1014 Poise
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.448866
@Wavelength 1128.950 nm
1.448866
@Wavelength 1128.950 nm
22°C, 1 atm, N2
 1.450241
@Wavelength 1014.26 nm
1.450241
@Wavelength 1014.26 nm
22°C, 1 atm, N2
 1.452463
@Wavelength 852.344 nm
1.452463
@Wavelength 852.344 nm
22°C, 1 atm, N2
 1.455144
@Wavelength 706.714 nm
1.455144
@Wavelength 706.714 nm
22°C, 1 atm, N2
 1.457016
@Wavelength 632.990 nm
1.457016
@Wavelength 632.990 nm
22°C, 1 atm, N2
 1.45846
@Wavelength 587.7250 nm
1.45846
@Wavelength 587.7250 nm
22°C, 1 atm, N2
 1.460076
@Wavelength 546.227 nm
1.460076
@Wavelength 546.227 nm
22°C, 1 atm, N2
 1.463123
@Wavelength 486.269 nm
1.463123
@Wavelength 486.269 nm
22°C, 1 atm, N2
 1.466691
@Wavelength 435.957 nm
1.466691
@Wavelength 435.957 nm
22°C, 1 atm, N2
 1.474539
@Wavelength 365.119 nm
1.474539
@Wavelength 365.119 nm
22°C, 1 atm, N2
 1.484493
@Wavelength 312.657 nm
1.484493
@Wavelength 312.657 nm
22°C, 1 atm, N2
 1.521154
@Wavelength 228.872 nm
1.521154
@Wavelength 228.872 nm
22°C, 1 atm, N2
 1.542665
@Wavelength 206.266 nm
1.542665
@Wavelength 206.266 nm
22°C, 1 atm, N2
 1.558918
@Wavelength 194.227 nm
1.558918
@Wavelength 194.227 nm
22°C, 1 atm, N2
Abbe Number 67.667.6Ve
 67.867.8Vd
Optical Dispersion 0.0067970.006797nF'-nC'
Transmission, Visible >= 99 %
@Wavelength 375 - 800 nm
>= 99 %
@Wavelength 375 - 800 nm
IR Transmittance  0.00 %
@Wavelength 2750 nm
0.00 %
@Wavelength 2750 nm
 0.00 %
@Wavelength 4300 nm
0.00 %
@Wavelength 4300 nm
 12 %
@Wavelength 4000 nm
12 %
@Wavelength 4000 nm
 65 %
@Wavelength 2200 nm
65 %
@Wavelength 2200 nm
 70 %
@Wavelength 3500 nm
70 %
@Wavelength 3500 nm
 88 %
@Wavelength 3400 nm
88 %
@Wavelength 3400 nm
 >= 99 %
@Wavelength 1500 nm
>= 99 %
@Wavelength 1500 nm
 >= 99 %
@Wavelength 1000 nm
>= 99 %
@Wavelength 1000 nm
UV Transmittance  99.8 %
@Wavelength 200 nm
99.8 %
@Wavelength 200 nm
 >= 99.9 %
@Wavelength 250 - 380 nm
>= 99.9 %
@Wavelength 250 - 380 nm
 >= 99.90 %
@Thickness 10.0 mm,
Wavelength 248 nm
>= 99.90 %
@Thickness 0.394 in,
Wavelength 248 nm
Internal Transmittance Ti > 99.90 %/cm
 
Descriptive Properties
Birefringence < 1 nm/cm(lower upon request)
Homogeneity GradeAA, A, C, F
Inclusion Class0, 1, 2
Metallic Impurities< 500 ppb
OH Content800 - 1000 ppm
Optical Stress Coefficient35.0 nm/cm MPa
Striae Class5ISO 10110-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCORNG09p / 281585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.