MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. The Cell Classification was determined using the notched Izod test with injection molded samples.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Hardness, Shore D 787815 sec; ASTM D2240
Tensile Strength, Yield 42.7 MPa6190 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.69 GPa390 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiASTM D790
Compressive Strength 55.8 MPa8090 psiASTM D695
Izod Impact, Notched  0.590 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
1.11 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Compression Molded; ASTM D256A
 0.850 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
1.59 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Compression Molded; ASTM D256A
 9.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy  35.6 J/cm
@Temperature 23.0 °C
0.0667 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 35.6 J/cm
@Temperature 23.0 °C
0.0667 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
ASTM D150
 3.9
@Frequency 60 Hz
3.9
@Frequency 60 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm686 kV/inASTM D149
Dissipation Factor  0.029
@Frequency 60 Hz,
Temperature 30.0 °C
0.029
@Frequency 60 Hz,
Temperature 86.0 °F
24 hr; ASTM D150
 0.040
@Frequency 1000 Hz,
Temperature 30.0 °C
0.040
@Frequency 1000 Hz,
Temperature 86.0 °F
24 hr; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C37.2 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
163 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 0.711 mm
V-0
@Thickness 0.0280 in
ALL; UL 94
 V-0
@Thickness 0.870 mm
V-0
@Thickness 0.0343 in
All Colors
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 179 - 182 °C354 - 360 °F
 
Descriptive Properties
Agency RatingsNSF 51
 NSF 61
Automotive SpecificationsCHRYSLER MS-DC28 Type B CPN2647 Color: Black
 GM GM7001M (PVC)
Ease of SizingExcellent
FeaturesGeneral Purpose
 Good Dimensional Stability
 Good Melt Strength
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16344ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Beltline Moldings
 General Purpose
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 83510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid

PH0POL0016 / 144585

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.