MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) LURAN KR 2635 Styrene Acrylonitrile Copolymer
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Base Polymer: Styrene/Acrylonitrile/Copolymer

Filler/Additive System: Silicone Oil

For use in: Acrylonitrile/Butadiene/Styrene/Copolymer, Styrene/Acrylonitrile/Copolymer, Acrylonitrile/Styrene/Acrylate/Copolymer

Special Features: High flow, slip agent, improved sliding/wear

Market Segment: Furniture, Building and Construction, Sport and Leisure

Applications Area: Injection molded parts, blow molded parts, extruded parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Drying Temperature  80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
air circulating dryer
 
Descriptive Properties
Base PolymerStyrene/Acrylonitrile/Copolymer
Dosage (%)5Extrusion
 5Injection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond Centrex® 825 Sheet Extrusion Grade
Elix Polymers ELIX ABS E401 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade
Mocom (ALBIS) ALTECH® ASA A 1000/128 UV ASA
Overview of materials for Styrene Acrylonitrile (SAN), Molded
Tabriz SH-0150 Extrusion Grade ABS

PALBIS8918 / 242977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.