MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cosmic Plastics ID-50 Dacron Filled Diallyl Iso-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP)

Material Notes: Description: Cosmic ID-50 is a Dacron-filled, general purpose diallyl ortho-phthalate molding compound which is supplied in a granular form. It molds easily in standard compression or transfer equipment.

Features: It has excellent electrical properties with an impact strength considerably higher than orlon filled material. A special processing enables ID-50 to retain its excellent volume and surface resistance after prolonged exposure to elevated temperature and 100% humidity.

Applications: The inherent strength of Dacron fibers makes this compound excellent for applications requiring high physical and/or electrical properties.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/cc
Bulk Factor 3.03.0
Water Absorption 0.35 %
@Temperature 50.0 °C,
Time 173000 sec
0.35 %
@Temperature 122 °F,
Time 48.0 hour
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.1 - 35.9 MPa3500 - 5200 psi
Flexural Strength 68.9 - 82.7 MPa10000 - 12000 psi
Compressive Strength 124 - 172 MPa18000 - 25000 psi
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm
 1.00e+10 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
1.00e+10 ohm-cm
@Temperature 158 °F,
Time 720 hour
100% RH
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohm
 1.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
1.00e+10 ohm
@Temperature 158 °F,
Time 720 hour
100% RH
Dielectric Constant  3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
Dry
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
Dry
 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
Wet
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
Wet
Dielectric Strength 13.8 kV/mm350 kV/inWet, step by step
 14.2 kV/mm360 kV/inDry, step by step
Dielectric Breakdown 50 V50 VWet, step by step
 62 V62 VDry, step by step
Dissipation Factor  0.0050
@Frequency 1000 Hz
0.0050
@Frequency 1000 Hz
Dry
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Dry
 0.015
@Frequency 1000 Hz
0.015
@Frequency 1000 Hz
Wet
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
Wet
Arc Resistance 115 sec115 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature -40.0 - 100 °C
22.2 µin/in-°F
@Temperature -40.0 - 212 °F
Heat Distortion Temperature 260 °C500 °F
 
Processing PropertiesMetricEnglishComments
Mold Temperature 135 - 190 °C275 - 374 °F
 
Descriptive Properties
Dimensional Stability<0.06%
MIL-M-14SDI-30ASTM D5948-96
Molding Pressure500-8000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cosmic Plastics 224 Dacron Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Sumitomo Bakelite RX® 647 Phenolic Resole Compound
Raschig Group 6501 DAIP

PCOSM010 / 190792

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.