MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Lustran® 456 Extrusion, Matte-Gloss  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with <10% orientation.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow 1.2 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.2 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6868ASTM D785
Tensile Strength, Yield 13.0 MPa1890 psiASTM D638
Tensile Modulus 1.00 GPa145 ksiASTM D638
Flexural Yield Strength 28.3 MPa4100 psiASTM D790
Flexural Modulus 1.20 GPa174 ksiASTM D790
Izod Impact, Notched 1.90 J/cm
@Thickness 3.17 mm
3.56 ft-lb/in
@Thickness 0.125 in
ASTM D256
 0.900 J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
1.69 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Impact Test 38.0 J
@Thickness 2.50 mm
28.0 ft-lb
@Thickness 0.0984 in
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 95.0 µm/m-°C
@Temperature 20.0 °C
52.8 µin/in-°F
@Temperature 68.0 °F
Injection molded sample; ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
@Thickness 3.17 mm
192 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 3.17 mm
176 °F
@Thickness 0.125 in
Unannealed; ASTM D648
UL RTI, Electrical 60.0 °C
@Thickness 1.60 mm
140 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical with Impact 60.0 °C
@Thickness 1.60 mm
140 °F
@Thickness 0.0630 in
UL746B
UL RTI, Mechanical without Impact 60.0 °C
@Thickness 1.60 mm
140 °F
@Thickness 0.0630 in
UL746B
Flammability, UL94  HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
 
Optical PropertiesMetricEnglishComments
Gloss <= 10 %<= 10 %60°; Sheet; ASTM D523
Transmission, Visible 0.00 %0.00 %Opaque only
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 - 240 °C419 - 464 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
Ineos ABS Lustran® ABS M406
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade
Ineos ABS Lustran® ABS E112LG Pellets
Ineos ABS Lustran® 130

PB1L13 / 26489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.