MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes: Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire test up to 960°C.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.4 %2.0 - 2.4 %23°C; 50% RH; ISO 62
Viscosity Measurement 130130ISO 307
Melt Flow 157.2 g/10 min
@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 2.70 GPa392 ksiISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °FInjection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry)
BASF Ultramid® C3U10 PA6/66 FR (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Dry, 30% Glass Filled, High Flow
Envalior Akulon® Ultraflow K-FPG8 PA6-I-GF40, Dry, 40% Glass Filled, High Flow

PBASG0331 / 131964

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.