Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax BR 713 N is a 20% talc filled PP copolymer, with high flowability, good impact/stiffness balance, good surface appearance and very good UV resistance. Applications: Automotive Parts, Exterior Trim. |