Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing an advanced system of lubrication. It has been develop
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPOM, Polyoxymethylene