MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Mindel® B-430 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 30% Glass Fiber Reinforced

Material Notes: Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically for electrical/electronic applications requiring flame resistance, but where flame retardant systems based on polybrominated diphenyl- oxides or ethers are undesirable. The resin has a UL 94 V0 rating at 0.062" (1.57 mm) thickness, even though it does not contain polybrominated diphenyl- ethers or oxides. This material can therefore be used in areas of the world where the use of flame retardants based on polybrominated diphenylethers/ oxides may be restricted. Mindel B-430 resin's resistance to warping results from low isotropic shrinkage. Combined with high stiffness, good creep resistance and high heat distortion temperature, Mindel B-430 resin may be ideally suited for use in demanding electrical components such as relays, switches, motor starters and control housings. Mindel B-430 resin should also be considered for electrical connectors that do not have the demanding temperature requirements of surface mount technology. The material has excellent regrind stability and, unlike polyesters, retains a high level of mechanical and electrical properties even at elevated temperatures and humidities. - Black: Mindel B-430 BK 174 - Natural: Mindel B-430 NT - Grey: Mindel B-430 GY 674 - Custom Colorable

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Filler Content, Glass Fiber
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Comparative Tracking Index, UL 746
  • Comparative Tracking Index, UL 746, PLC 3
  • Hot Wire Ignition, HWI, UL 746
  • Hot Wire Ignition, HWI, UL 746, PLC 0
  • High Voltage Arc-Tracking Rate, HVTR, UL 746
  • High Voltage Arc-Tracking Rate, HVTR, UL 746, PLC 0
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • UL RTI, Electrical, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical without Impact, UL 746
  • Flammability, UL94, UL 94
  • Melt Temperature
  • Drying Temperature
  • Injection Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.