Adflex 7635 XCP is a thermoplastic polyolefin, which is mainly used by our customers for the extrusion of blown film. It is also suitable for sheet extrusion. Adflex 7635 XCP features very high softness and very low modulus. It does not contain any slip or anti-blocking agents. Adflex 7635 XCP is used for the production of soft hygienic film and heavy duty film, as well as for the modification of LDPE or LLDPE to increase mechanical characteristics, puncture resistance, and to allow further downgauging. It can be easily processed on conventional LDPE or LLDPE blown film lines. Applications:
Agriculture Film, Bags & Pouches, Barrier Film, Breathable Film, Collapsible Tubes, Film Wrap, Food Packaging Film, Heavy Duty Packaging, Hygiene Film, Interior Automotive Applications, Lamination Film, Shrink Film, Stretch Hood, Surface Protection Film, TPO Foils and Skins. |