MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP31 High Shear and Peel Strength Room Temperature Curing Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Convenient handling
  • Excellent structural adhesive
  • Combines low viscosity and optical clarity
  • Provides superior electrical insulation values
Product Description: Master Bond EP31 is a two part epoxy system used primarily for bonding, but is also serviceable as a coating, sealing and encapsulation agent. The processing is relatively easy and straightforward with a forgiving mix ratio of 100 to 30 by weight. It cures readily at room temperature or more rapidly at elevated temperatures. At ambient temperatures, it cures in about 1-2 days, and at 200°F, in about 2-3 hours. To optimize properties, an overnight cure at room temperature followed by 2-3 hours at 150-200°F is desirable. Upon cross linking, EP31 has toughness and resiliency allowing it to withstand aggressive thermal cycling. Most prominent is its remarkable tensile lap shear and peel strength (summarized below). It bonds well to a wide variety of substrates, including metals, composites, glass, rubber, ceramics and many plastics. Some other desirable attributes include chemical resistance to water, oils and fuels; very good optical clarity and low shrinkage upon curing. It is a first class electrical insulator, which, when combined with its good flow properties, enables it to be used for smaller potting applications. The service temperature range is -60°F to +250°F. It is also available in a non-drip version called EP31ND. This robust product profile allows EP31 to be considered for use in aerospace, electronic, optical, opto-electronic, specialty OEM and related industries.

Product Advantages:

  • User friendly handling and processing
  • Versatile cure schedules
  • Stellar lap shear and peel strength properties
  • Top notch electrical insulation properties
  • Impressive optical clarity

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.