ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled sheets. As a result of its extremely low thermal expansion, ROBAX® can be subjected to extreme temperature differences. Even when used in high temperature conditions, ROBAX® maintains excellent stability of form. ROBAX® can be further processed mechanically using all of the normal methods of glass processing. Applications: ROBAX® possesses a high degree of resistance against thermal stresses and chemical surface attacks. Its diverse range of applications include: chemical process sight glass, high temperature vision windows, heat insulators, commercial ovens/broilers, architectural and outdoor lighting, electronics and UV light wave blocking applications. Information provided by SCHOTT North America. |