MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Westlake Mxsten CV77520 Polyethylene Plastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Mxsten CV Plastomer CV77520 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin exhibit exceptionally low seal initiation temperature with a broad hot tack window combined with good stiffness. Other features of this resin include extreme strength in cold and refrigerated temperature environments, high resistance to tears, and high MVTR.

    Application/Uses
  • Agricultural tubing
  • Blown film
  • Food packaging
  • Trash bags

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Exceptionally low seal initiation temperature with a broad hot tack window combined with good stiffness
Vendors:
Available Properties
  • Density, ASTM D1505
  • Thickness
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Elmendorf Tear Strength MD, ASTM D1922
  • Elmendorf Tear Strength TD, ASTM D1922
  • Dart Drop, ASTM D1709A
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Heat Seal Strength Initiation Temperature, Westlake
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, at 45º
  • Melt Temperature
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Westlake Chemical Corporation

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.