Butene Copolymer Features: - Excellent processability
- Outstanding balance of stiffness, cold temperature impact, toughness and ESCR
- Good organoleptic properties and color
Additives: Applications: - Bulk food, industrial and lubricant shipping pails
- Caps and closures
- Bins and totes
United States: SCLAIR 2807 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability. NOVA Chemicals polyethylene resins are biologically and chemically inert. Information provided by NOVA Chemicals® |