MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Saint-Gobain Tygon® LP 1200 Small Engine Fuel Transfer Tubing
Categories: Polymer; Thermoplastic

Material Notes: A low-permeation fuel tubing, the patent-pending Tygon® LP-1200 provides multiple solutions and benefits to some of the key challenges facing both outdoor power equipment OEMs and maintenance dealers such as easier assembly, ethanol compatibility and quicker diagnosis of fuel problems during service.

Applications

  • Handheld lawn and garden tools: chainsaws, brush cutters, trimmers, blowers
  • Fuel transfer hoses: lawn mowers, snow blowers, other ground supported equipment

Features and Benefits

  • Transparent
  • Quick diagnosis of fuel flow or leak issues
  • High purity fluoropolymer inner liner
  • Eliminates risk of rubber distractible contamination in carburetors
  • Superior chemical resistance and compatible with 100% ethanol fuel transfer
  • Worry free operation
  • Excellent fitting retention
  • 100% seal and optimum safety
  • Superior flexibility
  • Easy assembly, routing and optimized fuel pick up
  • Excellent elasticity
  • Prevents "necking" from over-stretching during installation
  • Submersible
  • Applicable with most fuel applications
  • UV resistant
  • Durable longer service life
  • EPA and CARB approved (Carb # Q-14-03)
  • Meets low permeation standards of 15g/m2/day
  • Patent pending
  • Proprietary design to differentiate
  • Choices of size and color
  • Custom to OEM needs

Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Tear Strength, ASTM D1004
  • Compression Set, ASTM D395, Method B
  • Tensile Set, ASTM D412
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air, Flexibility
  • Brittleness Temperature, ASTM D746-98, Impact
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.