MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Mitsubishi Chemical Advanced Materials Borotron® UH PE-UHMW + boron based additive (ISO Data)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very suitable for slowing down fast neutrons to lower energy thermal (slow) neutrons, which are then absorbed by the added boron compound. Whereas both PE-HMW and PE-UHMW are suitable for neutron shielding, PE-UHMW is often preferred because of its better deformation behaviour at high temperatures and its superior impact strength and wear resistance

  • Effectively attenuates neutron radiation particles and minimises the gamma radiation released during their capture
  • Very good wear and abrasion resistance
  • High impact strength (particularly PE-UHMW)
  • Excellent chemical resistance
  • Low coefficient of friction
  • Very low water absorption
  • Moderate mechanical strength, stiffness and creep resistance
  • Excellent machinability

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Outgassing - Total Mass Loss
  • Hardness, Shore D
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength, Yield, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Yield, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Flexural Strength
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • Compressive Strength, ISO 604
  • K Factor (ISO)
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 179-1/1eA, Partial Break
  • Coefficient of Friction, Dynamic
  • Sand Slurry
  • Limiting Pressure Velocity, at 1 m/s unlubricated
  • Limiting Pressure Velocity, at 0.1 m/s unlubricated
  • Volume Resistivity, IEC 60093
  • Surface Resistivity per Square, IEC 60093
  • CTE, linear
  • Thermal Conductivity
  • Melting Point, ISO 11357-1/-3, DSC, 10°C/min.
  • Maximum Service Temperature, Air, Continuous
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2
  • 3A-Dairy
  • European Food 1935/2004
  • FDA
  • USP Class VI
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsubishi Chemical Advanced Materials (former Quadrant Engineering Plastics Products)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.