MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
ITW Chockfast® PHILLYMASTIC TG-7B Epoxy Chocking Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYMASTIC TG-7B is a two-component, load-bearing, epoxy mastic specifically developed for LPG/LNG tank or container system installations where shimming or void-filling of supporting components is required. TG-7B provides excellent load-bearing and adhesive properties at cryogenic temperatures assuring evenly distributed loads across all tank supports. This mastic is available as either a liquid or a paste so it can be poured, pumped or troweled into place. Both the liquid and paste can be mixed either by hand or with automatic dispensing equipment. Phillymastic TG-7B was designed to meet the requirements set forth by GAZ Transport’s Technical Specification N. 402; Revision F issued in 1993 for LNG tank installation.

Thixotropy: Will not sag more than 10mm before hardening; sample TG-7B paste 60mm Wx100 mm Lx20mm D placed vertically at 20°C. ASTM D-2730.

Information provided by ITW Performance Polymers.

Vendors:
Available Properties
  • Specific Gravity, Paste
  • Specific Gravity, Liquid
  • Viscosity, Liquid. LIQUID TG-7B.
  • Viscosity, Mix. LIQUID TG-7B.
  • Viscosity, Resin. LIQUID TG-7B.
  • Hardness, Barcol, ASTM D2583, Paste
  • Hardness, Barcol, ASTM D2583, Liquid
  • Elongation at Break
  • Compressive Strength, ASTM D695, Liquid
  • Compressive Strength, ASTM D695, Paste
  • Compressive Modulus, ASTM D695, Liquid
  • Compressive Modulus, ASTM D695, Paste
  • Shear Strength, ASTM D732, Paste; Punch Shear Strength
  • Shear Strength, DIN EN 1465, Paste
  • Adhesive Bond Strength, ASTM D-1002, To birch wood. Plywood failure.
  • Adhesive Bond Strength, ASTM D-1002, To birch wood. Plywood failure.
  • Adhesive Bond Strength, ASTM D-1002, To birch wood. Plywood failure.
  • Adhesive Bond Strength, ASTM D-1002, To steel with shop primer. Adhesive to primer interface failure.
  • Adhesive Bond Strength, ASTM D-1002, To steel with shop primer. Adhesive to primer interface failure.
  • Adhesive Bond Strength, ASTM D-1002, To steel with shop primer. Adhesive to primer interface failure.
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM D2566, 0.001 inch per inch
  • Cure Time, approximate
  • Cure Time, approximate
  • Cure Time, approximate
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.