Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CA1110 G3 PO 1740 BLK is a high melt flow, medium high modulus, UV-stabilized, mineral filled thermoplastic elastomeric olefin (TEO) resin that has a good combination of properties and processability. It is typically used for unpainted automotive bumper fascia applications. Applications: Automotive Parts, Bumpers |