MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Latrobe LSS™ 135M Nitriding Steel (ASTM A355 Class A)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured from this steel are surface nitrided. The result is a nitrided surface which exhibits high hardness and good resistance to abrasion and wear, along with a strong and tough inner core in the piece. TLS 135M is supplied in the prehardened condition at a hardness of approximately 28 to 32 Rockwell C. In this condition, tools can be machined or ground, and then nitrided. Additional heat treatment is normally not required. Typical applications for TLS 135M steel include injection and extrusion feed screws, machine parts, pump parts, bushings, shafts, pinions, crankshafts, cams, camshafts, gears, valve sleeves, chuck jaws, dowel pins, and thread guides.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Hardness, Rockwell C, 5 inches; Mid-Radius
  • Hardness, Rockwell C, 3 inches; Mid-Radius
  • Hardness, Rockwell C, 5 inches; Surface
  • Hardness, Rockwell C, 3 inches; Surface
  • Hardness, Rockwell C, Up to 1.5 inches; Un-Nitrided
  • Tensile Strength, Ultimate, 5 inches; Un-Nitrided
  • Tensile Strength, Ultimate, 3 inches; Un-Nitrided
  • Tensile Strength, Ultimate, Up to 1.5 inches; Un-Nitrided
  • Tensile Strength, Yield, 5 inches; Un-Nitrided
  • Tensile Strength, Yield, 3 inches; Un-Nitrided
  • Tensile Strength, Yield, Up to 1.5 inches; Un-Nitrided
  • Modulus of Elasticity
  • Machinability, 1% Carbon Steel
  • CTE, linear
  • Thermal Conductivity
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Latrobe Steel

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.