High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2. Applications: Pump Impellers, Valve Housings and Bushings Processing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F) Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation. |