Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material exceeds the performance required by the automotive industry for polymeric materials exposed to antifreeze at 226°F (108°C), even when tested at 275°F (135°C). Potential applications include a variety of automotive components such as thermostat housings, heater core endcaps, heater hose connectors, and water inlets, outlets and valves. - Black: AS-1933 HS BK 324 Key Attributes: Antifreeze Resistant; Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Glycol Resistance; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength Applications: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts Automotive Specifications: ASTM D4000 PA121 G35 Color: BK324 Black; ASTM D6779 PA121G35; BMW GS 93016 Color: BK 324 Black; BOSCH N28 BN05-OX1 BN0510-GF45-3Gsw01SO Color: BK324 Black; CHRYSLER MS-DB-478 CPN4116 Color: Black; FORD WSS-M4D861-A3 Color: BK324 Black; GM GMP.PPA.019 Color: Black; GM GMW16360P-PPA-GF35 Color: BK-324 Black; ISO 1874 PA6T/6I/66, MH, 12-120, GF33 Color: BK324 Black; PSA Peugeot-Citroën SPA X62 4203; VALEO PDT NVB 10 057 Color: BK324 Black Injection Notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. Manufacturer recommendeds that Amodel® resins be dried prior to molding. Information provided by Solvay Specialty Polymers. |