Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CA 197 J WHITE is a medium melt flow, unfilled, polypropylene copolymer. The product is designed for continuous service at high temperature. This grade is available in white, in pellet form. Applications: Pipe Coating |