Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and do not outgas after curing. They are also environmentally safe, non-flammable materials which contain no volatile organic compounds. General Features: Bonds Plated Metals to Ceramic Bonding: Ceramic to Metal Principal Use: Heaters, Igniters, Gasketing |