MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Stratasys® Ultem 9085 for Rapid Prototyping
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM™ 9085 resin filament is a PEI (polyetherimide) thermoplastic FDM material. It features a high strength-to-weight ratio, high thermal and chemical resistance, and meets multiple aerospace and railway industry standards for flame, smoke and toxicity (FST) characteristics. ULTEM™ 9085 resin CG (Certified Grade) meets more stringent test criteria and possesses documented traceability from filament back to raw material lot number. Included documentation:
  • Certificate of Analysis – for both raw material and filament are supplied, documenting test results and identification to match filament manufacturing lot number to raw material batch number.
  • Certificate of Conformance – confirms that the material is manufactured in compliance to approved Stratasys and industry specifications.
Typical applications include production parts and functional prototypes. Available colors are natural and black.

Information provided by Stratasys.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792, XY, XZ/ZX Orientations
  • Tensile Strength at Break, ASTM D638, ZX Orientation, Black T16 tip
  • Tensile Strength at Break, ASTM D638, ZX Orientation, T20 tip
  • Tensile Strength at Break, ASTM D638, ZX Orientation, T16 tip
  • Tensile Strength at Break, ASTM D638, XZ Orientation, T16 tip
  • Tensile Strength at Break, ASTM D638, XZ Orientation, T20 tip
  • Tensile Strength at Break, ASTM D638, XZ Orientation, Black T16 tip
  • Tensile Strength, Ultimate, ASTM D638, ZX Orientation, T16A tip
  • Tensile Strength, Ultimate, ASTM D638, XZ Orientation, T16A tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, T20 tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, Black T16 tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, T16 tip
  • Tensile Strength, Yield, ASTM D638, ZX Orientation, T16A tip
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, T16A tip
  • Elongation at Break, ASTM D638, ZX Orientation, T16 tip
  • Elongation at Break, ASTM D638, ZX Orientation, Black T16 tip
  • Elongation at Break, ASTM D638, ZX Orientation, T20 tip
  • Elongation at Break, ASTM D638, XZ Orientation, Black T16 tip
  • Elongation at Break, ASTM D638, XZ Orientation, T16 tip
  • Elongation at Break, ASTM D638, XZ Orientation, T20 tip
  • Elongation at Yield, ASTM D638, XZ Orientation, T16 tip
  • Elongation at Yield, ASTM D638, XZ Orientation, Black T16 tip
  • Elongation at Yield, ASTM D638, XZ Orientation, T20 tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, T20 tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, T20 tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, Black T16 tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, T16 tip
  • Modulus of Elasticity, ASTM D638, ZX Orientation, T16A tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, T16 tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, Black T16 tip
  • Modulus of Elasticity, ASTM D638, XZ Orientation, T16A tip
  • Flexural Strength, ASTM D790, Procedure A, ZX Orientation, T16 tip
  • Flexural Strength, ASTM D790, Procedure A, ZX Orientation, T20 tip
  • Flexural Strength, ASTM D638, ZX Orientation, Black T16 tip
  • Flexural Strength, ASTM D790, Procedure A, Ultimate, ZX Orientation, T16A tip
  • Flexural Strength, ASTM D790, Procedure A, Ultimate, XZ Orientation, T16A tip
  • Flexural Strength, ASTM D790, Procedure A, XZ Orientation, T16 tip
  • Flexural Strength, ASTM D790, Procedure A, XZ Orientation, T20 tip
  • Flexural Strength, ASTM D638, XZ Orientation, Black T16 tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, T20 tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, Black T16 tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, T16 tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, T20 tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, T16 tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, Black T16 tip
  • Flexural Modulus, ASTM D790, Procedure A, XZ Orientation, T16A tip
  • Flexural Modulus, ASTM D790, Procedure A, ZX Orientation, T16A tip
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation, T20 tip
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation, T16 tip
  • Flexural Strain at Break, ASTM D790, Procedure A, ZX Orientation, Black T16 tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, T20 tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, Black T16 tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, T16 tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, T20 tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, T16 tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, Black T16 tip
  • Compressive Yield Strength, ASTM D695, XZ Orientation, T16A tip
  • Compressive Yield Strength, ASTM D695, ZX Orientation, T16A tip
  • Compressive Modulus, ASTM D695, XZ Orientation, T20 tip
  • Compressive Modulus, ASTM D695, XZ Orientation, T16 tip
  • Compressive Modulus, ASTM D695, XZ Orientation, Black T16 tip
  • Compressive Modulus, ASTM D695, ZX Orientation, T16 tip
  • Compressive Modulus, ASTM D695, ZX Orientation, T20 tip
  • Compressive Modulus, ASTM D695, ZX Orientation, Black T16 tip
  • Compressive Modulus, ASTM D695, XZ Orientation, T16A tip
  • Compressive Modulus, ASTM D695, ZX Orientation, T16A tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, T20 tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, T20 tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, Black T16 tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, T16 tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, ZX Orientation, T16A tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, T16A tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, T16 tip
  • Izod Impact, Notched, ASTM D256, ASTM D4812, XZ Orientation, Black T16 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation, T20 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation, T20 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation, Black T16 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, ZX Orientation, T16 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation, T16 tip
  • Izod Impact, Unnotched, ASTM D256, ASTM D4812, XZ Orientation, Black T16 tip
  • Volume Resistivity, ASTM D257, XY, XZ/ZX Orientations
  • Dielectric Constant, ASTM D150, XY, XZ/ZX Orientations
  • Dielectric Constant, ASTM D150, XY, XZ/ZX Orientations
  • Dissipation Factor, ASTM D150, XY, XZ/ZX Orientations
  • Dissipation Factor, ASTM D150, XY, XZ/ZX Orientations
  • CTE, linear, ASTM E831, XY, XZ/ZX Orientations
  • CTE, linear, ASTM E831, XY, XZ/ZX Orientations
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648 Method B, XY, XZ/ZX Orientations
  • Glass Transition Temp, Tg, ASTM D7426, Inflection Point, XY, XZ/ZX
  • Flammability, UL94, ANSI/UL 746B, Blue Card #E345258
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.