MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond MasterSil 800 One Component, Room Temperature Curing Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temperature resistance and non-corrosive cure, making it highly desirable for many applications, especially those pertaining to electronics and aerospace. MasterSil 800 is self leveling and bonds well to a wide variety of substrates, including glass, metals and many plastics. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. It is extremely soft with superb flexibility and elasticity and outstanding electrical insulation properties. MasterSil 800 is serviceable over the exceptionally broad temperature range of -75°F to +572°F (300°C). What is truly remarkable about the higher temperature range is that unlike other temperature resistant silicones (e.g. red silicones), MasterSil 800 will not depolymerize when exposed to 300°C and high pressure. In a sense, it can be considered a second generation high temperature resistant RTV. MasterSil 800 has a moderate viscosity, but is still flowable and is black in color.

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity
  • Hardness, Shore A
  • Tensile Strength
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Tensile Strength, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Elongation at Break, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Tensile Lap, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Adhesive Bond Strength, Heat Resistance, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Tack-Free Time
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.