MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and most stable zirconia material. Type FBD is ideally suited for thermal insulation and protection applications under conditions of ultra-high temperatures and in varied atmospheres. FBD has been high fired and is tightly bonded resulting in nearly dust free use. This tight bonding makes machining to tight tolerances possible.

FBD is dimensionally stable to 2000°C and can be used at higher temperatures in areas where some sintering can be tolerated. FBD has good hot strength up to 1700°C and can be used as a self supporting setter for loads equal to twice its own weight up to this temperature. It has exceptional resistance to oxidizing and reducing atmospheres at high temperatures. Zirconia does, however, lose a small amount of oxygen at very high temperatures in vacuum and inert or reducing atmospheres. Although this reaction results in a color change from white to gray, other properties remain essentially unchanged and insulation effectiveness is not impaired.

FBD has exceptional resistance to most corrosive environments. It undergoes little attack by molten alkali metal chlorides and carbonates at temperatures as high as 700°C and withstands aqueous solutions of alkali metal hydroxides at temperatures as high as 230°C. FBD will tolerate exposure to inorganic acids at their boiling point for short lengths of time. FBD contains no organic binders, produces no smoke or odor and undergoes no physically disruptive phase transitions when heated.

Features:

  • Rigid and Machinable
  • Our Most Dense, Highest Strength, Fibrous Zirconia Material
  • High Purity Zirconia Bonded
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Low Thermal Conductivity
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Surface Hardened with Zircar Zirconia Rigidizer Type ZR-RIG
  • Pre-fired and Organic Free

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors:
Available Properties
  • Bulk Density
  • Porosity
  • Outgassing - Total Mass Loss, In vacuum
  • Flexural Strength, Parallel to thickness
  • Compressive Yield Strength, Parallel to thickness @ 10% compression
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Softening Point, Dilatometric @ 10psi
  • Shrinkage, perpendicular to thickness
  • Shrinkage, perpendicular to thickness
  • Shrinkage, perpendicular to thickness
  • HfO2
  • Y2O3
  • ZrO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.