MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Parker Chomerics PREMIERâ„¢ PEI-140 High Temperature Conductive Plastic for EMI Shielding
Categories: Polymer

Material Notes: PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effectiveness, high temperature performance, low smoke generation, chemical resistance and UL 94V-0 flammability rating combined with a weight savings of 50-75%, make using PEI-140 for aerospace applications economically viable. PEI-140 specific gravity is 40% less than aluminum and 80% less than steel. PEI-140 offers an opportunity to reduce the weight of airborne electronic housings by up to 75%. PEI-140 housings will not only cost less themselves, but also improve aircraft operating cost through weight reduction.

Information provided by Chomerics

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Linear Mold Shrinkage, ASTM D995
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D412
  • Izod Impact, Unnotched, ASTM D412
  • Impact, ASTM D6110-05a, [ft-lb/in], Charpy
  • Surface Resistance
  • Surface Resistivity per Square, MIL-DTL-83528C
  • Shielding Effectiveness, ASTM D4935
  • Shielding Effectiveness, ASTM D4935
  • Shielding Effectiveness, ASTM D4935
  • Shielding Effectiveness, ASTM D4935
  • Shielding Effectiveness, IEEE 299
  • Thermal Conductivity, ASTM D5470
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • Smoke Density, BSS 7238/7239, NBS Ds
  • Oxygen Index, ASTM D2863, Limited
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Dry Time, Typical
  • Dry Time, Maximum
  • Moisture Content, Suggested Maximum
  • Back Pressure
  • Clamp Pressure, [MPa/cm2]
  • Cushion
  • Screw Speed, 760 - 1000 cm/min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.