Available Properties |
---|
- Specific Gravity, ASTM D792
- Density, ISO 1183
- Linear Mold Shrinkage, Flow, SABIC Method, 48 hrs @ 23°C, flow
- Linear Mold Shrinkage, Flow, SABIC Method, 1 hr @ 80°C, flow
- Linear Mold Shrinkage, Flow, SABIC Method, 30 min @ 120°C, flow
- Linear Mold Shrinkage, Transverse, SABIC Method, 48 hrs @ 23°C, xflow
- Linear Mold Shrinkage, Transverse, SABIC Method, 1 hr @ 80°C, xflow
- Linear Mold Shrinkage, Transverse, SABIC Method, 30 min @ 120°C, xflow
- Melt Flow, ISO 1133
- Hardness, Shore D, ISO 868
- Tensile Strength at Break, ASTM D638, Type I, 50 mm/min
- Tensile Strength at Break, ISO 527, 50 mm/min, 1A
- Tensile Strength, Yield, ASTM D638, Type I, 50 mm/min
- Tensile Strength, Yield, ISO 527, 50 mm/min
- Elongation at Break, ISO 527, 50 mm/min
- Elongation at Break, ASTM D638, Type I, 50 mm/min
- Elongation at Yield, ISO 527, 50 mm/min
- Elongation at Yield, ASTM D638, Type I, 50 mm/min
- Tensile Modulus, ISO 527, 1 mm/min
- Tensile Modulus, ASTM D638, 50 mm/min
- Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
- Flexural Modulus, ISO 178, 2 mm/min, 64mm span
- Izod Impact, Notched, ASTM D256, 63.5*12.7*3.2mm, Cut
- Izod Impact, Unnotched, ASTM D4812, 63.5*12.7*3.2mm, Cut
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4mm, Cut
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4mm, Cut
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4mm, Cut
- Charpy Impact, Notched, ISO 179/1eA, 80*10*4mm, Cut
- Charpy Impact, Notched, ISO 179/1eA, 80*10*4mm, Cut
- Charpy Impact, Notched, ISO 179/1eA, 80*10*4mm, Cut
- Dart Drop, Total Energy, ASTM D3763, Instrumented Impact Energy @ peak, 6.6 m/s
- Dart Drop, Total Energy, ASTM D3763, Instrumented Impact Energy @ peak @ 2.2 m/s
- Dart Drop, Total Energy, ASTM D3763, Instrumented Impact Energy @ peak, -30°C @ 2.2 m/s
- CTE, linear, Parallel to Flow, ISO 11359-2
- CTE, linear, Transverse to Flow, ISO 11359-2
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1&2, 80*10*4mm, Cut
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1&2, 80*10*4mm, Cut
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Vicat Softening Point, ISO 306, 10N, 50°C/hr
|
| | |